dc.contributor.author | Varawut Tangpasuthadol | - |
dc.contributor.author | Amarawan Intasiri | - |
dc.contributor.other | Chulalongkorn University. Faculty of Science | - |
dc.contributor.other | Chulalongkorn University. Faculty of Science | - |
dc.date.accessioned | 2010-04-29T10:13:52Z | - |
dc.date.available | 2010-04-29T10:13:52Z | - |
dc.date.issued | 2005 | - |
dc.identifier.uri | http://cuir.car.chula.ac.th/handle/123456789/12609 | - |
dc.description.abstract | Beside carbon black, silica powder is the other important filler used to reinforce various colored rubber products. In order to improve the compatibility between silica particles and rubber phase, this work has focused on preparing an NR composite, reinforced by silica generated inside the NR matrix or ‘in situ’. The silica particle was formed by a sol-gel process of tetraethoxysilane (TEOS) dispersed in NR latex. The latex used was concentrated latex having 60% rubber content, and already contained water and ammonia, two ingredients needed for the sol-gel reaction. The conversion of TEOS to silica was close to 100% and the particles size was about 44 nm in diameter, determined by TEM. The silica particles scattered evenly in the rubber. A statistical analysis method, named ‘two-level factorial design’, was used to study the influence of the amount of TEOS, ammonia, and gelation time on the mechanical properties of the composite. Silica content as high as 19% was prepared successfully. The composite had a tensile modulus of 3.7 MPa and a tear strength value of 41 N/nm. It was also found that the composite containing in situ silica had a higher tensile modulus and tear strength than a composite that was prepared by conventionally mixing with silica power. | en |
dc.description.budget | 282,000 Baht | en |
dc.description.sponsorship | ทุนอุดหนุนการวิจัยจากงบประมาณแผ่นดิน ประจำปี 2547 | en |
dc.format.extent | 2943653 bytes | - |
dc.format.mimetype | application/pdf | - |
dc.language.iso | en | es |
dc.publisher | Chulalongkorn University | en |
dc.rights | Chulalongkorn University | en |
dc.subject | Rubber | en |
dc.subject | Latex | en |
dc.subject | Sol-gel | en |
dc.subject | Silica | en |
dc.title | Silica reinforement of natural rubber by sol-gel process in latex | en |
dc.title.alternative | การเพิ่มความแข็งแรงของยางพาราแบบใช้ซิลิกาโดยกระบวนการโซลเจลในลาเทกซ์ | en |
dc.type | Technical Report | es |
dc.email.author | [email protected] | - |
dc.email.author | [email protected] | - |
Appears in Collections: | Sci - Research Reports |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
Varawut_Silica.pdf | 2.87 MB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.